RESISTANCE OF THERMALLY MODIFIED <i>Eucalyptus grandis</i> W. Hill ex Maiden WOOD TO DETERIORATION BY DRY-WOOD TERMITES (<i>Cryptotermes</i> sp.)

Authors

  • Djeison Cesar Batista
  • Silvana Nisgoski
  • José Tarcísio da Silva Oliveira
  • Graciela Inês Bolzón de Muñiz
  • Juarez Benigno Paes

DOI:

https://doi.org/10.5902/1980509822766

Keywords:

thermal modification process, VAP HolzSysteme®, termites attack.

Abstract

ABSTRACT

There are currently in operation at least five major European industrial processes for wood thermal modification. They improve wood’s dimensional stability and decay resistance, but are not efficient against termites attack. In fact, there is little research about the effect of thermal modification on wood resistance to termites, whether subterranean or dry-wood termites. The aim of this study was to evaluate the effect of the Brazilian process of thermal modification (VAP HolzSysteme®) on the resistance of Eucalyptus grandis wood to attack by Cryptotermes sp. dry-wood termites. Five treatments were tested: natural eucalypt wood, thermally modified eucalypt wood at three final temperatures (140, 160 and 180 °C) and pine wood (control). The attack was evaluated in terms of mass loss, mean score of wear grades, number of holes and termites mortality, according to a Brazilian method proposed by the Technological Research Institute of São Paulo (IPT, 1980). Similarly to the European processes of thermal modification, the Brazilian VAP HolzSysteme® was not effective to improve wood resistance to dry-wood termites attack, at least in the evaluated conditions. 

Downloads

Download data is not yet available.

References

AMERICAN SOCIETY FOR TESTING AND MATERIALS (ASTM). ASTM D 2017: accelerated laboratory test of natural decay resistance of woods. Philadelphia, 2005.

AMERICAN SOCIETY FOR TESTING AND MATERIALS (ASTM). ASTM D 3345: laboratory evaluation of wood and other cellulosic materials for resistance to termites. Philadelphia, 2008.

ASSOCIAÇÃO BRASILEIRA DOS PRODUTORES DE FLORESTAS PLANTADAS (ABRAF). Anuário estatístico ABRAF 2013 ano base 2012. Brasília: ABRAF, 2013. 148 p.

BATISTA, D. C.; KLITZKE, R. J.; SANTOS, C. V. T. Densidade e retratibilidade da madeira de clones de três espécies de Eucalyptus [Basic density and retractibility of wood clones of three Eucalyptus species]. Ciência Florestal, Santa Maria, v. 20, n. 4, p. 665-674, 2010.

BATISTA, D. C.; TOMASELLI, I.; KLITZKE, R. J. Efeito do tempo e temperatura de modificação térmica na redução do inchamento máximo da madeira de Eucalyptus grandis Hill ex Maiden [Effect of time and temperature of thermal modification on the reduction of maximum swelling of Eucalyptus grandis Hill ex Maiden wood]. Ciência Florestal, Santa Maria, v. 21, n. 3, p. 533-540, 2011.

BAZYAR, B. Decay resistance and physical properties of oil heat treated aspen wood. BioResources, Raleigh, v. 7, n. 1, p. 696-705, 2012.

BRITO, J. O. et al. Densidade básica e retratibilidade da madeira de Eucalyptus grandis, submetida a diferentes temperaturas de termorretificação [The density and shrinkage behavior of Eucalyptus grandis wood submitted to different temperatures of thermoretification]. Cerne, Lavras, v. 12, n. 2, p. 182-188, 2006.

CALONEGO, F.W.; SEVERO, E.T.D.; FURTADO, E.L. Decay resistance of thermally-modified Eucalyptus grandis wood at 140°C, 160°C, 180°C, 200°C and 220°C. Bioresource Technology, Amsterdam, v.101, n.23, p. 9391-9394, 2010.

CALONEGO, F.W.; SEVERO, E.T.D.; BALLARIN, A.W. Physical and mechanical properties of thermally-modified wood from E. grandis. European Journal of Wood Products, Berlin, v.70, p. 453-460, 2012.

CAO, Y. et al. Evaluation of decay resistance for steam-heat-treated Wood. BioResources, Raleigh, v. 6, n. 4, p. 4696-4704, 2011.

CLAUSEN, C. A. Biodeterioration of wood. In: FOREST PRODUCTS LABORATORY. Wood Handbook: wood as an engineering material. Madison: United States Department of Agriculture, Forest Service, Forest Products Laboratory, 2010. p. 14-1 – 14-16.

DUBEY, M. K.; PANG, S.; WALKER, J. Changes in chemistry, color, dimensional stability and fungal resistance of Pinus radiata D.Don wood with oil heat-treatment. Holzforschung, Berlin, v. 66, n. 1, p. 49-57, 2012.

ESTEVES, B. M.; DOMINGOS, I.; PEREIRA, H. Improvement of technological quality of eucalypt wood by heat treatment in air at 170-200°C. Forest Products Journal, Madison, v. 57, n. 1/2, p. 47-52, 2007a.

ESTEVES, B. M. et al. Influence of steam heating on the properties of pine (Pinus pinaster) and eucalypt (Eucalyptus globulus) wood. Wood Science and Technology, Berlin, v. 41, n.3, p.193-207, 2007b.

FINNISH THERMOWOOD ASSOCIATION. ThermoWood® Handbook. Helsink: Finnish Thermowood Association, 2003. 66 p.

HAKKOU, M. et al. Investigations of the reasons for fungal durability of heat-treated beech wood. Polymer Degradation and Stability, Amsterdam, v. 91, n. 2, p. 393-397, 2006.

HILL, C. Wood Modification: chemical, thermal and other processes. West Sussex: John Wiley & Sons, 2006. 239p.

INSTITUTO DE PESQUISAS TECNOLÓGICAS DE SÃO PAULO (IPT). Publicação IPT N°1157/DIMAD: Parte D, D2: Ensaio acelerado de laboratório da resistência natural ou de madeira preservada ao ataque de térmitas do gênero Cryptotermes (fam. Kalotermitidae). São Paulo, 1980.

INSTITUTO DE PESQUISAS TECNOLÓGICAS DE SÃO PAULO (IPT). Disponível em: <http://www.ipt.br/informacoes_madeiras3.php?madeira=13>. Acesso em: 22/10/2013.

KAMDEM, D. P.; PIZZI, A.; JERMANNAUD, A. Durability of heat-treated wood. Holz als Roh-und Werkstoff, Berlin, v. 60, n. 1, p. 1-6, 2002.

LEKOUNOUGOU, S. et al. Effect of heat treatment on extracellular enzymatic activities involved in beech wood degradation. Wood Science and Technology, Berlin, v. 43, n. 3-4; p. 331-341, 2009.

MBURU, F.; DUMARÇAY. S.; HUBER, F.; PÉTRISSANS, M.; GÉRARDIN, P. Evaluation of thermally modified Grevillea robusta heartwood as an alternative to shortage of wood resource in Kenya: characterization of physicochemical properties and improvement of bio-resistance. Bioresource Technology, Amsterdam, v. 98, n. 18, p. 3478-3486, 2007.

MOHAREB, A. et al. Effect of heat treatment intensity on wood chemical composition and decay durability of Pinus patula. European Journal of Wood and Wood Products, Berlin, v. 70, n. 4, p. 519-524, 2012.

MOMOHARA, I.; OHMURA, W.; KATO, H.; KUBOJIMA, Y. Effect of high-temperature treatment on wood durability against the brown-rot fungus, Fomitopsis palustris, and the termite, Coptotermes formosanus. In: INTERNATIONAL IUFRO WOOD DRYING CONFERENCE, 8., 2003, Brasov. Proceedings… Brasov: “Transilvania” University of Brasov, 2003. p. 284-287.

OLIVEIRA, J. T. da S. Caracterização da madeira de eucalipto para a construção civil [Characterization of eucalyptus wood for construction]. 1998. 429 f. Tese (Doutorado em Engenharia) – Escola Politécnica, Universidade de São Paulo, São Paulo.

PESSOA, A.M. das C.; BERTI FILHO, E.; BRITO, J.O. Avaliação da madeira termorretificada de Eucalyptus grandis, submetida ao ataque de cupim de madeira seca, Cryptotermes brevis [Evaluation of the Eucalyptus grandis thermorectificated wood submitted to the drywood termite attack, Cryptotermes brevis]. Scientia Forestalis, Piracicaba, n.72, p. 11-16, 2006.

PLATOWOOD. Disponível em: <http://www.platowood.nl/languages/english>. Acesso em: 22/10/2013.

RETIWOOD. Disponível em: <http://www.retiwood.com>. Acesso em: 22/10/2013.

RIBEIRO JÚNIOR, J. I. Análises estatísticas no SAEG. Viçosa: UFV, 2001. 301p.

RILLING, E.A.G. Madeira modificada com calor: TMT – Thermally modified timber. Ponta Grossa, 2010. Informativo Técnico TW Brazil. Disponível em: <http://www.twbrazil.com.br/upload/arquivos/a8c4b18b0f.pdf>. Acesso em: 18/10/2013.

SILVA, J. de C.; LOPEZ, A. G. C.; OLIVEIRA, J. T. da S. Influência da idade na resistência natural da madeira de Eucalyptus grandis W. Hill ex Maiden ao ataque de cupim de madeira seca (Cryptotermes brevis) [Tree age influence on Eucalyptus grandis wood natural resistance to deterioration by dry-wood termites]. Árvore, Viçosa, v. 28, n. 4, p. 583-587, 2004.

SILVA, J. de C. et al. Variação da retratibilidade da madeira de Eucalyptus grandis Hill ex Maiden, em função da idade e posição radial no tronco [Influence of age and radial position the volumetric and linear shrinkage of Eucalyptus grandis Hill ex Maiden wood]. Árvore, Viçosa, v.30, n. 5, p. 803-810, 2006.

SPIEGEL, M. R. Estatística. 3. ed. São Paulo: Pearson Education do Brasil, 1994. 643.

STAMM, A. J. Wood and Cellulose Science. New York: The Ronald Press, 1964. 549 p.

Published

2016-06-20

How to Cite

Batista, D. C., Nisgoski, S., Oliveira, J. T. da S., Muñiz, G. I. B. de, & Paes, J. B. (2016). RESISTANCE OF THERMALLY MODIFIED <i>Eucalyptus grandis</i> W. Hill ex Maiden WOOD TO DETERIORATION BY DRY-WOOD TERMITES (<i>Cryptotermes</i> sp.). Ciência Florestal, 26(2), 671–678. https://doi.org/10.5902/1980509822766

Issue

Section

Technical Note

Most read articles by the same author(s)

1 2 3 4 > >>